LOCTITE® 660 - Tube 10.0/case High Strength Retaining Compound
Known as Loctite 660 Quick Metal, Press Fit Repair
Features and Benefits
Available sizes:
- High viscosity
- Ideal for use with worn parts without re-machining
- Registered to NSF Category P1
- Suitable for retaining shims
- Gap fill of 0.25mm-0.5mm (0.01"-0.02")
Documents and Downloads
- Tube 10.0/case - IDH 135527
Looking for a TDS or SDS in another language?
Technical Information
Agency approvals / certificates / specifications | NSF P1 |
Application method | Manual |
Applications | Press fitting, Repairing, Retaining |
Color | Silver |
Cure type | Anaerobic cure |
Fixture time | 15.0 min. |
Gap fill | 0.25 - 0.5 mm |
Key characteristics | Gap filling, Strength: high strength, Thixotropic |
Operating temperature | -65.0 - 300.0 °F (-55.0 - 150.0 °C ) |
Physical form | Paste |
Recommended for use with | Metal: steel |
Shear strength, Steel | 23.0 N/mm² (3335.0 psi ) |
Viscosity | 250000.0 mPa·s (cP) |
How to
Step by Step Guide
1. Preparation - Cleaning
Use LOCTITE SF 790 to remove any old adhesive from parts. Use LOCTITE SF 7070 to degrease and clean surfaces prior to applying adhesive. For gaps larger than 0.5mm or worn out shafts, bearing seats or keyways, use LOCTITE metal-filled compounds to rebuild the surfaces.
2. Preparation - Activation
If cure speed is too slow due to passive metals (stainless steel, aluminum and plated metals) or low temperature (below 5°C), use LOCTITE SF 7649 activator. Allow to dry.
3. Application - For Slip-Fitted Assemblies
Apply adhesive around the leading edge of the male component and the inside of the female component. Assemble parts with a rotating motion to ensure good coverage. Wipe off excess adhesive.
4. Application - For Press-Fitted Assemblies
Apply 360 degree beads of adhesive to both bond surfaces at the leading edges of insertion or engagement, and assemble at high press-on rates. Wipe off excess adhesive.
5. Application - For Shrink-Fitted Assemblies
Apply the adhesive onto the male component, heat the female component to cause expansion for free assembly. Assemble components and allow temperatures to equiliberiate. Wipe of excess adhesive.
6. Disassembly
Apply localized heat to approximately 500°F/260°C and disassemble while hot.